PVC Solvent Cement
ASTM International D-2564:
The ASTM D-2564 covers requirements for PVC solvent cements used in PVC piping Systems.
Key Requirements Of This Standards Are:
- Lap shear strength – 62 Bar after 72 hour curing time.
- Hydro-static burst strength -27 Bar after 2 hours curing time.
- Resin Content
- Dissolution
- Viscosity
Low VOC:
VOC – Volatile Organic Compounds, Less than 510 grams per liter. Ideal for use in green building construction.
Shelf Life & Storage:
The date code of manufacturing is printed on the bottom of each tin. Evaporation of solvent will cause the cement to thicken and reduce its effectiveness. Adding thinners / solvents to change viscosity is not recommended and may significantly change the properties of the cement. Store between 5°C and 44 °C